BigPatents India

 
 

NICKEL ALLOY AND METHOD OF DIRECT AGING HEAT TREATMENT

3909/KOLNP/2007 A (3909/KOLNP/2007)

Filed on 2007-10-12

Publication date 2008-05-30

Embodiments of the present disclosure relate to nickel-base alloys and methods of direct aging nickel-base alloys. More specifically, certain embodiments of the present disclosure relate to methods of direct aging 718PlusĀ® nickel-base alloy to impart improved mechanical properties, such as, but not limited to, tensile strength, yield strength, low cycle fatigue, fatigue crack growth, and creep and rupture life to the alloys. Other embodiments of the present disclosure relate to direct aged 718PlusĀ® nickel-base alloy, and articles of manufacture made therefrom, having improved mechanical properties, such as, but not limited to, tensile strength, yield strength, low cycle fatigue, fatigue crack growth, and creep and rupture life.

Applicant

ATI PROPERTIES, INC.
1600 NE OLD SALEM ROAD, POST OFFICE BOX: 460, ALBANY, OR U.S.A.

Inventor

KENNEDY RICHARD L., CAO WEI-DI

International Information

Classification
C22F 1/10
Publication number
WO 2007/084178
Application date
2006-05-09
Application number
PCT/US2006/017804

View application at Intellectual Property India

 
 
HomeApplications → 3909/KOLNP/2007 A
 
 

Applications


Names

Granted Patents


Subscriptions


Other

 
BigPatents India was developed with generous funding from the Ford Foundation
Created by XB Labs | Contact Us | Disclaimer