A PROCESS FOR PREPARING POLYESTER

Application 840/CAL/1999 published 2006-01-13, filed 1999-10-12
A process is disclosed for the preparation of a polyester polymer or polyester copolymer under superatmospheric pressure conditions in a pipe or tubular reaction under turbannular flow conditions. Reaction material having a glycol equivalents to carboxylic acid equivalents mole ratio of from 1.0:1 to 1.2:1, together with a superatmospheric dense gaseous medium are fed co-currently to the reactor. Dicarboxylic acid and\or diol raw materials may be injected into any of the reaction zones in the process during operation to achieve the overall desired mole ratio balance. The process operates at temperatures of from about 220 0C to about 320 0C, with turbannular flow achieved before the polymer product and gas exit the reactor process. The pressure in the reaction zones can be in the range from 15 psia to 2500 psia. A polymer product having a DP of a greater than 40, more preferably at least about 70, is achieved by the transfer of water from the reacting material polymer melt to the gaseous medium in the reactor. (FIG.Nil)

Applicant

ARTEVA TECHNOLOGIES S.A.R.L.,
LUXEMBOURG, TALSTRASSE 80, 8001 ZURICH, SWITZERLAND.

Inventor

MAURER CHARLES J. SHAW GORDON SMITH VICKY S.

International Info

Classification: C08F 2/00, 6/00

Priority Information

09/185,998 USA 1998-11-04