CRYSTALLIZABLE THERMOPLASTIC RESINS AND DENDRIMERS WITH IMPROVED FABRICATION CHARACTERISTICS

Application 24/MUMNP/2006 published 2006-09-01, filed 2006-01-05
The strain-hardening characteristics and melt rheology of thermoplastic resins including crystallizable polyester resins are modified by blending with a dendrimeric modifier. Blends comprising PET resins and up to about 2 wt.% of a dendrimer have increased melt strengths and exhibit a reduction in strain-hardening parameter, reflected in a lower strain level at the onset of strain hardening. Blends further comprise PET resins and a component comprising a ratio of dendrimer modifier to purified terephthalic acid. Drawing: 5 Sheets Total Pages: 31 Fig. 1

Applicant

BP CORPORATION NORTH AMERICA INC.
4101 WINFIELD ROAD, WARRENVILLE, IL 60555, U.S.A.

Inventor

1. DAIRANIEH ISSAM 2. RUBIS DONALD E.

International Info

Classification: C08L 67/00, C08G 63/08, C08L 101/00
Publication Number: WO 2004/111126
Application Date: 2004-06-10

Priority Information

60/477,731 U.S.A. 2003-06-11